Premix Thermoplastics PREADD AB 576

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Premix Thermoplastics Inc.
Trade Name PREADD
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PREADD AB 576.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PREADD AB 576 is a polypropylene based antiblock masterbatch developed especially for polypropylene cast and blown films.PREADD AB 576 is based on highly purified synthetic silica. Due to its excellent dispersion in the masterbatch the antiblocking effect can be achieved already at relatively low dosing levels. PREADD AB 576 does not affect the transparency of the film at given addition levels. PREADD AB 576 can also be used at higher dosing levels as an antislip and a matting agent. PREADD AB 576 is approved for use in contact with foodstuffs according to FDA regulations without limitations and according to BgVV regulations as long as the dosage level of PREADD AB 576 is less than 6 %.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
Additive Loading 10 %
10 %
Synthetic Silica
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Carrier PP Homo Polymer
Color Whitish
Dosing, % 0.5 to 2
For Antiblock Effect
10 to 40
For Matting
2 to 5
For Antislip Effect
Light Fastness 8-Very Good