Material Notes:
Low Compression Set, Grey Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compression set grade, offering excellent heat resistance and low temperature flexibility. Used primarily for dry heat static seals, low physical strength and poor abrasion resistance prevents dynamic sealing.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
60 - 80
60 - 80
°IRHD, ±10 change after 70 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 4.275 MPa
620.0 psi
-25% change after 70 hours @ 200°C; ASTM D412
5.70 MPa
827 psi
ASTM D412
Elongation at Break 82.5 %
82.5 %
-45% change after 70 hours @ 200°C; ASTM D412
150 %
150 %
ASTM D412
Compression Set 15 %
15 %
24 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
-60.0 °C
-76.0 °F
Non-brittle after 3 minutes
Flash Point >= 300 °C
>= 572 °F