Material Notes:
Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Extruded onlyRoHS CompliantInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.70 - 2.20 g/cc
1.70 - 2.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 80
60 - 80
ASTM D2240
Tensile Strength >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break <= 200 %
<= 200 %
ASTM D412
Tear Strength <= 9.64 kN/m
<= 55.0 pli
ASTM D624
Compression Set <= 35 %

@Temperature 100 °C,
Time 252000 sec
<= 35 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.50 ohm-cm
<= 0.50 ohm-cm
without pressure-sensitive adhesive; MIL-DTL-83528
Shielding Effectiveness >= 75 dB

@Frequency 1.00e+8 Hz
>= 75 dB

@Frequency 1.00e+8 Hz
E-Field; Method 3, CHO-TM-TP09
>= 85 dB

@Frequency 1.00e+10 Hz
>= 85 dB

@Frequency 1.00e+10 Hz
Plane Wave; Method 3, CHO-TM-TP09
>= 105 dB

@Frequency 2.00e+9 Hz
>= 105 dB

@Frequency 2.00e+9 Hz
Plane Wave; Method 3, CHO-TM-TP09
Descriptive Properties Value Comments
Binder EPDM
Filler Ni/C
Heat Aging <0.35 ohm-cm
MIL-DTL-83528 Para. 4.6.15