| Category | Carbon , Graphite |
| Manufacturer | Ohio Carbon Blank |
| Trade Name | OCB |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Ohio Carbon Blank OCB TTK-4C EDM Grade Graphite.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Apparent Bulk Density | 2.90 g/cc | 0.105 lb/in³ | |
| Particle Size | 4.1 µm | 4.1 µm | Average |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 60 | 60 | |
| Tensile Strength | 60.6 MPa | 8790 psi | |
| Flexural Strength | 107 MPa | 15500 psi | |
| Compressive Strength | 193 MPa | 28000 psi |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.000254 ohm-cm | 0.000254 ohm-cm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Grain | Ultra-Fine | |
| Suggested Applications | Forging Dies | |
| Large Cavity Molds | ||
| Large Die Casts | ||
| Large Extrusion Dies | ||
| Roughing Electrodes | ||
| Wear Resistance | Very Good |