Oceanchem Group Triethyl Phosphate (TEP)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Triethyl Phosphate (TEP).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Molecular Formula: (CH3CH2O)3POCas No.: 78-51-3Use: Flammable inhibitor of rubber and plastic; raw material for pesticide, hardener and stabilizer of resin.Characteristics: It can dissolve in water wholely, it is easy to dissolve in organic solvent, such as ethyl alcohol, ether, benzene and others.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Specific Gravity 1.069 - 1.073 g/cc
1.069 - 1.073 g/cc
D2020
Processing Properties Metric English Comments
Moisture Content 0.20 %
0.20 %
Descriptive Properties Value Comments
Acidity 0.05
mg KOH/g; Reagent (export degree)
0.1
mg KOH/g; Industrial Grade
Appearance Colorless transparent liquid
CAS Number 78-51-3
Chroma 20
APHA
Content (%) 96
Industrial Degree
99.5
Reagent (export degree)
Dioptric Raten D20 1.403-1.406
Industrial Degree
1.405-1.407
Reagent (export degree)
Molecular Formula (CH3CH2O)3PO