Material Notes:
Molecular Formula: KCOOHInformation Provided by Oceanchem Group
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Descriptive Properties Value Comments
Content (%) 96-98
Molecular Formula KCOOH
Potassium Carbonate (%) <1
Potassium Chloride (%) <2