Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Objet FullCure® 830 Vero White Resin for Rapid Prototyping

Category Polymer , Rapid Prototyping Polymer
Manufacturer Objet
Trade Name FullCure®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Objet FullCure® 830 Vero White Resin for Rapid Prototyping.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by American Precision Prototyping, LLC
Physical Properties Metric English Comments
Water Absorption at Saturation 1.47 %
1.47 %
ASTM D570-98
Ash <= 0.40 %
<= 0.40 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81
81
Hardness, Shore D 83
83
Tensile Strength, Ultimate 49.8 MPa
7220 psi
ASTM D638-03
Elongation at Break 20 %
20 %
ASTM D412
Tensile Modulus 2.495 GPa
361.9 ksi
ASTM D638-04
Flexural Strength 74.6 MPa
10800 psi
ASTM D790-03
Flexural Modulus 2.137 GPa
309.9 ksi
ASTM D790-04
Izod Impact, Notched 0.241 J/cm
0.451 ft-lb/in
ASTM D256-06
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 47.6 °C
118 °F
ASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 43.6 °C
110 °F
ASTM D648-06
Glass Transition Temp, Tg 58.0 °C
136 °F
DMA, E"