Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Northstar Polymers MPG-023 Isocyanate Prepolymer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Northstar Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers MPG-023 Isocyanate Prepolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.112 g/cc
1.112 g/cc
Viscosity 1000 - 1400 cP

@Temperature 25.0 °C
1000 - 1400 cP

@Temperature 77.0 °F
Descriptive Properties Value Comments
Amine Equivalents 225.9
Appearance at 25°C Liquid
NCO (%) 18.6
Users viewing this material also viewed the following: