NAPCO Brown Fused Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer NAPCO
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NAPCO Brown Fused Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Premium grade of fused alumina produced by a top quality producer of alumina in China. Data provided by the manufacturer, North American Processing Company.
Mechanical Properties Metric English Comments
Knoop Microhardness 2000 - 2200
2000 - 2200
Hardness, Mohs 9.0
9.0
Component Elements Properties Metric English Comments
Al2O3 96.34 %
96.34 %
CaO 0.15 %
0.15 %
Fe2O3 0.080 %
0.080 %
MgO 0.50 %
0.50 %
SiO2 0.56 %
0.56 %
TiO2 2.65 %
2.65 %