Multibase Multibatch® ME 50008 Anti-blocking Masterbatch

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Multibase
Trade Name Multibatch®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Multibase Multibatch® ME 50008 Anti-blocking Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LDPE. 70% Silicate Filled. Clarity IRInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO R 1183
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 190 °C
20 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133