Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Monmouth Rubber & Plastics Durafoamâ„¢ S88 PVC/NBR

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Monmouth Rubber & Plastics
Trade Name Durafoam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Monmouth Rubber & Plastics Durafoamâ„¢ S88 PVC/NBR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.0961 g/cc
0.00347 lb/in³
ASTM D1056
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D1667
<= 5.0 %
<= 5.0 %
ASTM D1056
Linear Mold Shrinkage <= 0.050 cm/cm

@Temperature 70.0 °C,
Time 605000 sec
<= 0.050 in/in

@Temperature 158 °F,
Time 168 hour
Mechanical Properties Metric English Comments
Hardness, Shore OO 50
50
Tensile Strength >= 0.827 MPa
>= 120 psi
ASTM D412
Elongation at Break >= 175 %
>= 175 %
ASTM D412
Compressive Strength 0.0448 MPa
6.50 psi
Deflection @ 25%; ASTM D1056
Compression Set <= 25 %
<= 25 %
0.5; ASTM D1056
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -23.3 °C
-10.0 °F
Minimum Service Temperature, Air 107 °C
225 °F
Descriptive Properties Value Comments
C/D Heat Aging <30%
7 days @ 158°F, ASTM D1056
Color Grey
Fluid Immersion <50%
ASTM D1056
Ozone Resistance 0
72 hrs @ 50 pphm, ASTM D1171
Resilience 12-18%
(1/2" thk. @ 72ºF) Bashore (% Rebounded Average)