Momentive Performance Materials FQE206U Heat Cured Fluorosilicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials FQE206U Heat Cured Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.Fluorosilicones are suitable for applications in presence of fuel, oils, blow by gas, and various solvents. FQE206U is a peroxide curable, low compression set grade silicone elastomer.All Fluorosilicones are available as customized ready-to-use products.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Tensile Strength 11.2 MPa
1620 psi
Elongation at Break 280 %
280 %
Tear Strength 125 kN/m
713 pli
Die B
Compression Set 5.0 %
5.0 %
Descriptive Properties Value Comments
Appearance Light Yellow