Michelman® Michem® Emulsion 93935 Nonionic polyethylene emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 93935 Nonionic polyethylene emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 93935 is a phenol and formaldehyde free wax emulsion used mainly in floor polish formulations where it imparts black heel resistance, toughness and buffability and mar and scuff resistance.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamWhen manufactured in Belgium product meets food contact regulations for: Germany: BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in Belgium: FDA:175.105: Components of adhesives.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 64.5 - 65.5 %
64.5 - 65.5 %
pH >= 7.0
>= 7.0
Recommended pH of system
9.0 - 10.5
9.0 - 10.5
Brookfield Viscosity <= 50 cP
<= 50 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Translucent liquid
Emulsifier Charge Nonionic
Solids Type High Density Polyethylene