Material Notes:
Data provided by The Matrixx Group, formerly RePlas.
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
73°F; ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 145 MPa
21000 psi
0.125 in; ASTM D638
Flexural Modulus 8.62 GPa
1250 ksi
Tangent, 0.125 in; ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
0.125 in, 73°F; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Relative Thermal Index; UL746
Deflection Temperature at 0.46 MPa (66 psi) 234 °C
453 °F
0.125 in; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
0.125 in; ASTM D 648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in