Material Notes:
Master Bond UV18Med is a new one component, high strength UV curable system with good chemical resistance and flexibility for coating, sealing and bonding. UV18Med meets USP Class VI specifications for medical applications.
Physical Properties Metric English Comments
Viscosity 1800 - 2000 cP

@Temperature 23.0 °C
1800 - 2000 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 60
55 - 60
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Transparent