Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Magyar Aluminum ALO-P95-06 Alumina

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Magyar Aluminium
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Magyar Aluminum ALO-P95-06 Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alumina for Polishing
Physical Properties Metric English Comments
Bulk Density 0.400 - 0.600 g/cc
0.0145 - 0.0217 lb/in³
Oil Absorption 30 - 40 %
30 - 40 %
ml/100g
Particle Size 4.0 - 8.0 µm
4.0 - 8.0 µm
d50
63 µm
63 µm
0.5% max, wet sieve
Specific Surface Area 3.0 - 8.0 m²/g
3.0 - 8.0 m²/g
BET
Component Elements Properties Metric English Comments
Al2O3 >= 99 %
>= 99 %
Fe2O3 <= 0.040 %
<= 0.040 %
Na2O <= 0.30 %
<= 0.30 %
SiO2 <= 0.040 %
<= 0.040 %
Descriptive Properties Value Comments
Calcination Degree Medium