Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs PD780 [Pd(NH3)4](NO3)2 Tetraminepalladium(II) nitrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PD780 [Pd(NH3)4](NO3)2 Tetraminepalladium(II) nitrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 298.53 g/mol
298.53 g/mol
Descriptive Properties Value Comments
Assay 36% Pd
CAS Number 13601-08-6
Form Pale yellow crystals
Purity 99.999%
Typical Impurities Ca = 3; Cu, Zn, Ag, Fe, Mg, Na, Pt < 1 ppm
Users viewing this material also viewed the following: