MV Labs CS700 CsNO3 Cesium nitrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF MV Labs CS700 CsNO3 Cesium nitrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 194.91 g/mol
194.91 g/mol
Descriptive Properties Value Comments
Assay 68% Cs
CAS Number 7789-18-6
Form White crystals
Purity 99.999%
Typical Impurities Rb = 5; K, Na = 1 ppm