Key Features: conventional melt flow, very high modulus, mineral-filled polypropylene homopolymer, excellent heat resistance, high stiffness, excellent chemical resistance, good surface qualityApplications: automotive components, small and large appliancesDescription: Astryn 65F4-3 conventional melt flow, 30% talc-filled polypropylene homopolymer is designed for high heat stability, high rigidity, excellent chemical resistance and improved surface quality of molded parts.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792B
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
ASTM D648