Lucite International Colacryl ® TS1414/4 Acrylic Solution Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® TS1414/4 Acrylic Solution Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible resin produced in a slow drying petroleum fraction and designed for printing inks and covercoats on ceramic and glass transfers. Colacryl® TS1414/4 is a butyl methacrylate copolymer system and has reasonable compatibility with medium and long oil alkyds and vinyl resins. The product is compatible with phthalate, sebacate, and maleate plasticisers.Suggested Uses:Recommended for use in silk screen printing inks and media for the ceramic industry.Information provided by Lucite International
Physical Properties Metric English Comments
Solids Content 50 %
50 %
Viscosity 20000 - 27500 cP
20000 - 27500 cP
Descriptive Properties Value Comments
Solvent Solvesso 1000