Lubriplate PM 500 White Oil USP Mineral -Based Food Machinery Grade

Category Fluid , Lubricant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate PM 500 White Oil USP Mineral -Based Food Machinery Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This oil contains emulsifying agents that wet the lubricated surfaces and provide an oily film for the moving parts. Used very successfully on pear machines.Available in Bottles, Jugs, Pails, 1/4 Drums and DrumsH-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 86
86
Viscosity Index
100
100
ISO Grade
Saybolt Viscosity at 100°F 560 SUS
560 SUS
Saybolt Viscosity at 210°F 64 SUS
64 SUS
Kinematic Viscosity at 40°C (104°F) 101 cSt
101 cSt
Kinematic Viscosity at 100°C (212°F) 11 cSt
11 cSt
Thermal Properties Metric English Comments
Pour Point -20.6 °C
-5.00 °F
Flammability Test 485
485
[°F] Fire Point
Flash Point 216 °C
420 °F
Descriptive Properties Value Comments
SAE Gear Oil No. 80
SAE No. 30