Lubriplate FGL 2 Aluminum Complex USP Mineral Oil-Based Food Machinery Grade Grease

Category Fluid , Lubricant , Aluminum Gellant
Manufacturer Lubriplate Lubricants
Trade Name FGL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate FGL 2 Aluminum Complex USP Mineral Oil-Based Food Machinery Grade Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance, multi-purpose food grade grease designed to meet the demands of food and beverage industry plant engineers who want Class H-1 greases to totally replace H-2 greases. Fortified with anti-wear, anti rust and anti-corrosion additives which combine to yield excellent shear stability, load carrying capability and resistance to water and caustic wash down. Available in four NLGI densities for a variety of applications. FGL-CC is for centralized/automatic lubrication systems on high speed can closing equipment.FGL Series greases are available in Cans, Pails, 1/4 Drums and Drums. FGL-1 and FGL-2 are available in Cartridges.H-1 Class Lubricants are manufactured with ingredients that comply with FDA regulation 21 CFR 178.3570 for lubricants with incidental contact with the edible product.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 850 SUS
850 SUS
Kinematic Viscosity at 40°C (104°F) 160 cSt
160 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 265
265
Unknown Amount of Work
Penetration P(60), 1/10 mm 295
295
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -12.2 °C
10.0 °F
Approx. Cold test
Dropping Point 268 °C
515 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW
NLGI Grade 2
Rust/Oxidative Additives YES
Water Resistant YES