Description: SBR 1502 is a cold polymerized styrene-butadiene copolymer with styrene content of 23.5%. SBR 1502, a general purpose SBR, exhibits the excellent tensile strength, abrasion resistance, flexibility and recovery properties that are characteristic of cold polymerized SBR. This non-staining, non-discoloring polymer offers a wide range of bright and colorful stocks capable of satisfying requirements in a variety of products.Applications: SBR 1502 can be used to white sidewall tires, shoe soles, light and dark colored industrial goods and miscellaneous items where excellent physical properties and discoloration are required. CAS No: 9003-55-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
Volatiles 0.30 %
0.30 %
Mooney Viscosity 52

@Temperature 100 °C
52

@Temperature 212 °F
ML 1+4
Ash 0.20 %
0.20 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.4 MPa

@Temperature 145 °C,
Time 2100 sec
4260 psi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
Elongation at Break 470 %

@Temperature 145 °C,
Time 2100 sec
470 %

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
300% Modulus 0.0181 GPa

@Temperature 145 °C,
Time 2100 sec
2.63 ksi

@Temperature 293 °F,
Time 0.583 hour
ASTM D412
Chemical Properties Metric English Comments
Styrene Content 23.5 %
23.5 %
Bound
Descriptive Properties Value Comments
Color Light Tan Bale
Components HAF
50, ASTM D3185
SBR 1500H
100, ASTM D3185
Stearic Acid
1, ASTM D3185
Sulfur
1.75, ASTM D3185
TBBS
1, ASTM D3185
ZnO
3, ASTM D3185
Organic Acid 0.028
Rheometer 16.5 min
t'90, 160°C, 1° Arc, ASTM D5289
2.5 min
ts1, 160°C, 1° Arc, ASTM D5289
32 lb-in
MH, 160°C, 1° Arc, ASTM D5289
4.0 lb-in
ML, 160°C, 1° Arc, ASTM D5289
8.7 min
t'50, 160°C, 1° Arc, ASTM D5289
Soap 0.001