LG Chemical PB1120 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical PB1120 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General Description: PB1120, homopolymer made by micro-suspension seeded polymerization, is medium-viscosity PVC resin with pseudo plastic flow property. It can be used for foam flooring layer and wall paper made by knife coating and rotary screen coating. Products made from PB1120 has excellent reformation and printing abilityMain Applications: Wall coverings for rotary screen, Foam layer for flooring, Synthetic leather.CAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.406 g/cc
1.406 g/cc
Bulk Density 0.310 - 0.410 g/cc
0.0112 - 0.0148 lb/in³
ASTM D1895
Volatiles <= 0.70 %

@Temperature 110 °C,
Time 3600 sec
<= 0.70 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Brookfield Viscosity 15000 - 45000 cP
15000 - 45000 cP
DOP 60phr; ASTM D1824
Viscosity Measurement >= 2.0
>= 2.0
[g/sec], DOP 60phr, Severs; ASTM D1823
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 950-1050
30°C, JIS K 6720-2
K-Value 66
DIN53726 / ISO1628-2