Kraton® G1701 H (SEP) Linear Diblock Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® G1701 H (SEP) Linear Diblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Kraton G1701 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form identified: Kraton G1701 HU - supplied as a powder.Region: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton G1701 H is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Packaging and Polymod; and Personal CareInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D4025
Volatiles <= 1.0 %
<= 1.0 %
BAM 907
Kinematic Viscosity at 100°C (212°F) 15 - 19 cSt
15 - 19 cSt
1.7%, ENJ404; BAM 1201
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 64

@Time 10.0 sec
64

@Time 0.00278 hour
Typical values on polymer compression molded at 350°F; ASTM D2240
Tensile Strength 2.07 MPa
300 psi
Typical properties of film cast from toluene solution; ASTM D412
Elongation at Break >= 100 %
>= 100 %
Typical properties of film cast from toluene solution.; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 100 %
100 %
Descriptive Properties Value Comments
Content Non-staining phenolic antioxidant
0.03-0.2%, BAM 929
Polystyrene
34.7-38.5%, Measured on the polymer before hydrogenation, BAM 919
Total Extractables
<3.0%, BAM 1206
Styrene/Rubber Ratio 37/63