Iran Petrochemical (PCC) Moplen EP-T30 U Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Moplen EP-T30 U Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Moplen EP-T30 U is a heterophasic copolymer for injection moulding applications. Moplen EP-T30 U combines outstanding processability with extremely high impact Resistance. Moplen EP-T 30 U is designed for applications where very high toughness is a primary requirement.Applications: injection molding boxes, containers, pallets, crates, pails, bitumen modification and various compounding applications.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 0.40 g/10 min
0.40 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Stress 22.0 MPa
3190 psi
ISO R527
Elongation at Yield 11 %
11 %
ISO R527
Flexural Modulus 0.950 GPa
138 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 141 °C
286 °F
ISO 306/A
Heat Distortion Temperature 85.0 °C
185 °F
ISO 75/B