IDI Composites M-205 Thermoset Polyester, Sheet

Category Polymer , Thermoset , Composite SMC , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer IDI Composites
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites M-205 Thermoset Polyester, Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Water Absorption 0.10 %
0.10 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
ASTM D2583
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Strength 193 MPa
28000 psi
ASTM D695
Izod Impact, Notched 8.20 J/cm
15.4 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149