Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ICO Polymers ICORENEâ„¢ 440-1312 PP Rotational Molding Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICORENE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICORENEâ„¢ 440-1312 PP Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: ICORENE 440-1312 is a polypropylene copolymer developed for rotational molding applications. The resin is fully UV protected. Key Characteristics: very high rigidity, good creep resistance, good high temperature resistance. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Index of Compound 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
50 mm/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
50 mm/min; ASTM D638
Tensile Modulus 1.20 GPa
174 ksi
1 mm/min; ASTM D638
Flexural Modulus 1.35 GPa
196 ksi
1.3 mm/min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648