Hexcel® Redux® 212-NA Foaming adhesive film

Category Polymer , Adhesive , Film
Manufacturer Hexcel
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Hexcel® Redux® 212-NA Foaming adhesive film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Redux 200 series is a range fo foaming adhesive films presented in sheet form. They expand during the cure cycle to fill gaps and adhere strongly to all parts of the structure with which they come into contact. Redux foaming adhesive films are compative with Redux film adhesives.Features: High strength at temperatures from -67°F to 428°F; Less than 1% volatiles emitted during cure; Suitable for aluminum and fiber-reinforced composite sandwich constructions; Expansion ratios from 1:1.9 to 1:4.0.Application: Low foaming ratio. Suitable for vacuum and non vacuum cure.Associated Film Adhesives: Redux 312, 335, 382H, 609, 610
Mechanical Properties Metric English Comments
Shear Strength 4.86 MPa

@Temperature 100 °C
705 psi

@Temperature 212 °F
Aluminum Double Lap Shear (0.06 inch gap)
8.494 MPa

@Temperature 22.2 °C
1232 psi

@Temperature 72.0 °F
Aluminum Double Lap Shear (0.06 inch gap)
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 121 °C
1.00 hour

@Temperature 250 °F
Heat up rate 10°F/min
Shelf Life 18.0 Month

@Temperature -17.8 °C
18.0 Month

@Temperature 0.000 °F