Hexcel® HexWeb® HRH-49 - 1/4 - 2.1 Woven Kevlar Honeycomb

Category Polymer , Thermoset , Aramid
Manufacturer Hexcel
Trade Name HexWeb®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® HRH-49 - 1/4 - 2.1 Woven Kevlar Honeycomb.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-49 is manufactured using KEVLAR® 49 fabric. A thermosetting adhesive is used for the node bonds and a 350°F cure modified epoxy resin is applied for initial and final impregnations. The standard cell size is 1/4 inch. Due to the low resin content of HexWeb® HRH-49, core movement may occur during handling and part curing if proper restraining techniques are not employed.Features: Lightweight; Excellent thermal stability; Very low coefficient of thermal expansion; Good flatwise tensile strength; Excellent dielectric properties.Applications: HexWeb® HRH-49 has been developed by Hexcel for use as a sandwich core material in radomes and antennas. When used with KEVLAR® 49 or graphite facings, the HexWeb® HRH-49 sandwich has been considered to have good thermal stability when exposed to cyclic heat exposures such as encountered in space applications.
Physical Properties Metric English Comments
Density 0.0336 g/cc
0.00122 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 0.689 MPa
>= 100 psi
Stabilized, min
0.896 MPa
130 psi
Stabilized
Compressive Modulus 0.172 GPa
25.0 ksi
Stabilized
Shear Modulus 0.00896 GPa
1.30 ksi
Plate Shear, W Direction
0.0186 GPa
2.70 ksi
Plate Shear, L Direction
Shear Strength >= 0.207 MPa
>= 30.0 psi
Plate Shear, W Direction, min
0.276 MPa
40.0 psi
Plate Shear, W Direction, typ
>= 0.345 MPa
>= 50.0 psi
Plate Shear, L Direction, min
0.586 MPa
85.0 psi
Plate Shear, L Direction, typ