Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexForce™ GA130 Carbon Fabric

Category Carbon , Carbon Fiber
Manufacturer Hexcel
Trade Name HexForce™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ GA130 Carbon Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When properly engineered, carbon fabric composites can achieve the strength and stiffness of metals at significant weight savings. Hexcel's carbon fabrics are compatible with various resin systems including epoxy, polyester and vinyl ester resins.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 429 microns
16.9 mil
Mechanical Properties Metric English Comments
Tensile Modulus 228 GPa
33000 ksi
12K Carbon Warp Yarn
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 13.2
Dry
Nominal Construction (count/in) 14
Warp
4
Fill
Weave Style Plain Heatset
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved