Hexcel® HexForce™ 7642 Fiber Glass Fabric

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ 7642 Fiber Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential allowing the end user to choose the best combination for material performance, economics and product flexibility.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 279 microns
11.0 mil
Mechanical Properties Metric English Comments
Tensile Impact 90.8 J/cm
170 ft-lb/in
Filling Breaking Strength
187 J/cm
350 ft-lb/in
Warp Breaking Strength
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 6.84
Dry
Nominal Construction (count/in) 20
Fill
44
Warp
Type of Yarn Fill Yarn: ECG 37 1/0 Tex
Warp Yarn: ECG 75 1/0
Weave Style Plain