Hexcel® HexForce™ 112 Fiber Glass Fabric

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ 112 Fiber Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential allowing the end user to choose the best combination for material performance, economics and product flexibility.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 81.3 microns
3.20 mil
Mechanical Properties Metric English Comments
Tensile Impact 48.1 J/cm
90.0 ft-lb/in
Filling Breaking Strength
64.1 J/cm
120 ft-lb/in
Warp Breaking Strength
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 2.1
Dry
Nominal Construction (count/in) 39
Fill
40
Warp
Type of Yarn Fill Yarn: ECD 450 1/2
Warp Yarn: ECD 450 1/2
Weave Style Plain