Material Notes:
This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 85
75 - 85
Tensile Strength >= 10.3 MPa
>= 1500 psi
12.4 MPa
1800 psi
Typical
Elongation at Break >= 125 %
>= 125 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -34.4 °C
-30.0 °F