Freudenberg Simrit Simriz® 483 Low Temperature FFKT Perfluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Freudenberg Simrit
Trade Name Simriz®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Freudenberg Simrit Simriz® 483 Low Temperature FFKT Perfluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of elasticity. Simriz® perfluoro elastomers close the material gap between inelastic PTFE and elastomers, which have poor temperature and chemical resistance properties. With a fluoridation level of 72%, FFKM elastomers have a level of resistance close to that of pure PTFE at 76%. At the same time, FFKM materials are so elastic that they are excellently suited to both static and dynamic seals. Simrit offers ISC O-Rings which are specifically optimised with respect to flexibility at low temperatures, resistance to high temperatures, hardness, tensile strength, elongation, compression set, or color.Information provided by Freudenburg-NOK.
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Tensile Strength, Ultimate 10.5 MPa
1520 psi
Elongation at Break 230 %
230 %
Compression Set 33 %

@Temperature 200 °C
33 %

@Temperature 392 °F
70 hr
Descriptive Properties Value Comments
Color White
Water Resistance 27
70 h; 200°C