Material Notes:
Features: Ultra high impact strength and long term heat aging.Applications: Injection molding and extrusion: high pressure resistance, film and flexible profilesInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.8 g/10 min
1.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 58
58
ASTM D785
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 13 %
13 %
ASTM D638
Flexural Modulus, 1% Secant 720 MPa
104000 psi
ASTM D790
Izod Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Gardner Impact >= 36.0 J

@Temperature -30.0 °C
>= 26.6 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 740 MPa
107000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648