Fainplast Compounds PM 8020 Flexible PVC, Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds PM 8020 Flexible PVC, Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Covering steel sheaths
Physical Properties Metric English Comments
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 76 - 80
76 - 80
ISO R 868
Tensile Strength at Break 18.0 MPa
2610 psi
ISO R 527
Elongation at Break 300 %
300 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -26.0 °C
-14.8 °F
Cold Flex; ISO 458/2