ELM® SoyGrease™ Premium Biodegradable Food Grade Grease, NLGI Grade 2

Category Fluid , Lubricant
Manufacturer ELM®
Trade Name SoyGrease™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELM® SoyGrease™ Premium Biodegradable Food Grade Grease, NLGI Grade 2.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Elm ELM SoyGrease™ Food Machinery is formulated with optimized USA grown natural seed oils that surpass the lubricity of most conventional oils. It is formulated in accordance with the criteria established by USDA H-1 and U.S. FDA regulation 21 CFR 178.3570, “Lubricants With Incidental Food Contact.” It has been approved by the NSF.Applications: Meets the demanding applications of the food processing and beverage industries. Excellent for lubrication of bearing, grease lubricated gears, and machine slidesBenefits: Superior lubricity protects moving parts Extreme pressure additives protect under heavy shock loads Protects all ferrous metal components from rust and corrosion Superior adhesion resists water wash out Excellent operating temperature range Meets USDA’s proposed Biobased product definition for EO 13101 Meets EPA’s Environmental Preferable Purchasing (EPP) criteria Made from renewable USA-grown crop-based oils Meets State of Iowa Senate File - SF 2185 and 2249 Information provided by ELM®
Physical Properties Metric English Comments
Viscosity Measurement 213
213
Base Oil, Index
Kinematic Viscosity at 40°C (104°F) 40 cSt
40 cSt
Kinematic Viscosity at 100°C (212°F) 8.6 cSt
8.6 cSt
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
Four Ball Wear 0.480 mm
0.0189 in
Penetration 280
280
Cone, worked 60 strokes; ASTM D217
Descriptive Properties Value Comments
Appearance Golden