Material Notes:
Solprene 200P is a medium cis polybutadiene partially branched to reduce cold flow and improve processability. Solprene 200P has excellent mixing and processing behavior, is used as ingredient for plastic modification specialty for polystyrene by “IN SITU” reaction. Also, the product can be used in other applications where good performance at low temperatures, excellent abrasion resistance, low heat build-up and good dynamic fatigue resistance are needed. Solprene 200P has an antioxidant system that offers excellent stability to gel formation and color. It is presented in bales wrapped in polystyrene film.Applications:Plastic modificationInformation provided by Dynasol
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D-297
Volatiles <= 0.75 %
<= 0.75 %
ASTM D-5668
Mooney Viscosity 47

@Temperature 100 °C
47

@Temperature 212 °F
ML (1 + 4); ASTM D-1646
Viscosity Measure 144 cSt
144 cSt
Styrene solution viscosity 5%; ASTM D-1416
Ash <= 0.20 %
<= 0.20 %
ASTM D-1416
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -92.0 °C
-134 °F
(DSC on set); NM 300-58
Descriptive Properties Value Comments
Color Alpha, max 3
Monsanto gel, grade max 3