Dymax 3-20556 Solvent-Free Plastic Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 3-20556 Solvent-Free Plastic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide variety of engineering plastics. Curing in seconds upon exposure to UV/visible light, these resins are ideal for bonding transparent surfaces and for potting, sealing, and coating applications. Ultra Light-Weld adhesives and sealants cure upon exposure to UV and/or visible light and are perfect for UV blocked and tinted plastics. Light Weld products cure upon exposure to UV light.Environmentally responsible, solvent free adhesives reduce regulatory compliance cost, and encourage worker acceptance of the assembly process.Dymax 3-20556 Solvent-Free Plastic Adhesive Key Substrates: General tacking (primary), FR-4, Fabric, Paper, Polycarbonate Typical Use: Moisture resistance
Physical Properties Metric English Comments
Viscosity 7300 cP
7300 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 26.2 MPa
3800 psi
Elongation at Break 50 %
50 %