Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This product is used for release films and is available in 500 gauge.Typical Applications: Tracing FilmLabelsStampingImagingInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 130 %
130 %
ASTM D882A
Film Elongation at Break, TD 110 %
110 %
ASTM D882A
Coefficient of Friction, Dynamic 0.32
0.32
ASTM D1894
Coefficient of Friction, Static 0.36
0.36
ASTM D1894
Film Tensile Strength at Break, MD 186.0 MPa
26970 psi
ASTM D882A
Film Tensile Strength at Break, TD 195.9 MPa
28420 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 0.90 %

@Temperature 150 °C,
Time 1800 sec
0.90 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.30 %

@Temperature 150 °C,
Time 1800 sec
0.30 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 92 %
92 %
ASTM D1003
Transmission, Visible 67 %
67 %
ASTM D1003