Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers VTR 8655 (GBL-S) , VTR 8650 8655/8650 Blend  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Performance Polymers VTR 8655 (GBL-S) , VTR 8650 8655/8650 Blend  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FormulationVTR 8655
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 20.1 MPa
2920 psi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 317 %
317 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Modulus of Elasticity 0.000800 GPa
0.116 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 0.00440 GPa
0.638 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 14 %

@Temperature 200 °C
14 %

@Temperature 392 °F
Method B, O-rings 22 hr at 200°C (Post Cured 4 hr at 232°C)
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -18.1 °C
-0.580 °F
MDSC, postcured