Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers VTR 8525 (GBLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Performance Polymers VTR 8525 (GBLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FormulationVTR-8525
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Tensile Strength, Ultimate 19.6 MPa
2840 psi
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Elongation at Break 222 %
222 %
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Modulus of Elasticity 0.000710 GPa
0.103 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 16 hr at 232°C
100% Modulus 0.00690 GPa
1.00 ksi
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Thermal Properties Metric English Comments
Brittleness Temperature -27.7 °C
-17.9 °F
TR-10, 100% Elongation
Glass Transition Temp, Tg -27.3 °C
-17.1 °F
DSC
Users viewing this material also viewed the following: