Dow Corning SYL-OFF® 7610 COATING

Category Other Engineering Material , Catalyst/Initiator , Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® 7610 COATING.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Syl-Off® 7610 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer. General purpose coating with exceptional thin-film bathlife.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Viscosity 370 cP
370 cP
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance colorless liquid