Material Notes:
An inverse (water in oil) emulsion of sodium polyacrylate in dimethicone (200 Fluid, 5 cSt) for use in skincare, suncare, hair care, and color cosmetic applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity <= 4000 cP
<= 4000 cP
dynamic
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
closed cup
Descriptive Properties Value Comments
Active Content (%) 29
Cyclotetrasiloxane Content (%) <1