Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Bayfit® High Density Polyurethane Flexible Molded Foam, High Density

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Covestro
Trade Name Bayfit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayfit® High Density Polyurethane Flexible Molded Foam, High Density.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 0.0480 g/cc
0.00173 lb/in³
Core Density, ASTM D3574
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.100 - 0.230 MPa
14.5 - 33.4 psi
ASTM D3574E
Elongation at Break 130 %
130 %
ASTM D3574E
Compression Set 6.0 - 12 %
6.0 - 12 %
Test D, ASTM D3574 Dry