ConocoPhillips Hydroclear® Automatic Transmission Fluid

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® Automatic Transmission Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear DEXRON® III & MERCON® Automatic Transmission Fluid is a multipurpose fluid for the electronically controlled transmissions of most domestic and imported automobiles, trucks and buses built after 1989. It is approved by GM as a DEXRON III fluid and by Ford as a MERCON fluid. It is recommended for Ford transmissions requiring Type CJ and Type H fluids. It is approved by Allison as a C-4 fluid and also can be used in off-highway transmissions, power steering systems and other hydraulic systems. Hydroclear DEXRON III & MERCON Automatic Transmission Fluid is suited for a wide variety of industrial applications that call for an ISO 46 or SAE 20W hydraulic fluid. It qualifies as a Denison HF-O hydraulic fluid and has performed well in both Sunstrand and Vickers hydraulic pumps. Hydroclear DEXRON III & MERCON Automatic Transmission Fluid improves shifting characteristics at both high- and low-ambient temperatures. It resists thermal and oxidative degradation and offers outstanding low-temperature fluidity. It inhibits the formation of gum, sludge, lacquer and foam, protecting transmission from rust, corrosion and wear. It is dyed red for easy identification.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 33.3 °
33.3 °
Viscosity 14900 cP

@Temperature -40.0 °C
14900 cP

@Temperature -40.0 °F
Viscosity Measurement 197
197
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 33 cSt
33 cSt
Kinematic Viscosity at 100°C (212°F) 7.7 cSt
7.7 cSt
Thermal Properties Metric English Comments
Pour Point -51.1 °C
-60.0 °F
Flash Point 190 °C
374 °F
Descriptive Properties Value Comments
Color Red