ConocoPhillips Hydroclear® 30 Power-D E.O. 30

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® 30 Power-D E.O. 30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corrosion. These performance- proven, heavy-duty engine oils are recommended for both on- and off-road service, including construction, forestry, mining, marine and stationary power generation. They are also recommended for propane and compressed natural gas engines. In Power-D Engine Oil, the exclusive combination of hydrocracked base oils and unique high-performance additives offer excellent soot control, which results in cleaner engines, longer engine life and fewer drain intervals. Hydroclear Power-D Engine Oil SAE 15W40 exceeds the performance requirements of API CH-4; Mack EO-M; EO-M Plus; Cummins CES 20071, 20072, 20076, and 20077; and Volvo VDS and VDS-2, as well as the top EUROPEAN specifications. Hydroclear Power-D Engine Oil, in the appropriate viscosity grades, is recommended for use in most domestic and imported heavy-duty engines.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 28.9 °
28.9 °
Viscosity Measurement 109
109
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 91 cSt
91 cSt
Kinematic Viscosity at 100°C (212°F) 11.1 cSt
11.1 cSt
Ash 1.35 %
1.35 %
Sulfur
ASTM Color 3.5
3.5
Thermal Properties Metric English Comments
Pour Point -33.9 °C
-29.0 °F
Flash Point 243 °C
469 °F
Chemical Properties Metric English Comments
Total Base Number 10.2
10.2