Colorite Polymers Vinylbond 95-950-50 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Colorite Polymers
Trade Name Vinylbond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Colorite Polymers Vinylbond 95-950-50 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to rigid CPVC which makes them ideal for coextrusion profile applications. These compounds are provided non-pigmented and are intended to be custom colored by the customer.Information provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Ultimate 4.91 MPa
712 psi
Elongation at Break 187 %
187 %
100% Modulus 0.00286 GPa
0.415 ksi