Chosun Refractories SAL95 Special High Alumina brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SAL95 Special High Alumina brick.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.20 g/cc
0.116 lb/in³
Porosity 14 %
14 %
Mechanical Properties Metric English Comments
Compressive Strength 98.1 MPa
14200 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.50 µm/m-°C

@Temperature 1000 °C
4.17 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1500 °C,
Time 7200 sec
0.00 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 96 %
96 %
Fe2O3 0.20 %
0.20 %
Descriptive Properties Value Comments
Main Application Ammonia plant, Carbon productor, Rotary kiln, Shaft kiln, Various high-temp. furnace
Refractories Under Load(2kg/?,T2?) 1,700 T2
Refractoriness (SK) 41